Characterization of Spot Welding Behavior by Dynamic Electrical Parameter Monitoring

Total Page:16

File Type:pdf, Size:1020Kb

Characterization of Spot Welding Behavior by Dynamic Electrical Parameter Monitoring Characterization of Spot Welding Behavior by Dynamic Electrical Parameter Monitoring The use of two parameters—dynamic resistance and critical expulsion energy—is proposed for controlling resistance spot welding BY D. W. DICKINSON, J. E. FRANKLIN AND A. STANYA ABSTRACT. A program was undertak­ obtained by comparing dynamic a continuous or dynamic monitoring en to develop techniques for studying resistance curves for various high system is needed. This system would the resistance spot welding process. A strength steels. monitor and record instantaneous dynamic electrical parameter monitor­ Expulsion is analyzed in terms of changes in the electrical functions ing device was designed to simulta­ power curves integrated to obtain during welding. neously record the instantaneous val­ total weld energy input. It was found Several authors156 report contin­ ues of voltage, current, power, and that expulsion occurs when the total uous variations in the electrical param­ resistance during spot welding. The useful energy into the weld exceeds a eters during welding of mild steel data obtained using this technique critical value. It is proposed that these sheet to be typified by the sketches have been analyzed in terms of the two parameters, dynamic resistance presented in Fig. 1. After approximate­ relationships of these parameters to and critical expulsion energy, can be ly the first cycle, an increase in voltage the phenomena occurring during the used to control the spot welding pro­ across the welding electrodes and a formation of a spot weld, to the effects cess. decrease in current flowing through of changes in welding variables on the weld zone occurs until a "peak electrical parameters, and to the Introduction region" is reached. Throughout the effects of variations in steel composi­ remaining portion of the weld cycle, tion and properties. It has long been known that the the voltage decreases to a constant The phenomena occurring during process of spot welding occurs value while the current increases to a spot weld formation (surface break­ through the localized melting and constant value. down, asperity collapse, heating of the coalescence of a small volume of These changes in voltage and cur­ work pieces, molten nugget formation, material due to the heating caused by rent can also be represented as instan­ nugget growth, and mechanical col­ the passage of electric current. This taneous or dynamic resistance. Several lapse) can be understood through heating is equivalent to the product of authors1,56 have calculated the dy­ analysis of dynamic resistance curves. the current squared times the total namic resistance changes throughout If expulsion occurs during a spot weld, resistance of the material to be spot the welding cycle by dividing the it also is readily detected from this welded. During the process of spot instantaneous voltage by the instanta­ parameter. A generalized resistance welding, however, both the current neous current (R = E/l). This dynamic curve consists of an initial very rapid and the resistance continually change resistance trace is also plotted in Fig. 1. drop in resistance to a minimum value as the material is heated and melts. After an initial drop, it too rises to a within the first few cycles of current Until recently, spot weld character­ peak in the first portion of the weld flow. This is followed by a rise to a istics have been determined by mea­ cycle, dropping off later in the cycle. maximum and finally a gradual de­ surement of the initial or static The appearance of this dynamic crease. resistance and the initial current surge resistance trace and hence the basic Dynamic resistance measurements at the onset of welding, or an average welding mechanisms can be altered by RMS current value obtained during changes in welding variables such as can be used in obtaining a better 6 understanding of lobe curves. The welding. Recent papers,'" however, weld time, electrode force, and overall shape of the dynamic resistance curve have indicated that in order to fully weld current. Bhattacharya and An­ 1 for welds near the lobe boundary is characterize the spot welding process, drews have made the following correlated to the observed characteris­ observations: tics of these welds. The effects of Based on a paper presented at the AWS 1. With low current values, the changes in welding current and elec­ 60th Annual Meeting held in Detroit, resistance trace does not show a prom­ trode force can also be related to the Michigan, during April 2-6, 1979. inent peak; with increased welding dynamic resistance curves. Spot weld­ current, however, a well-defined peak D. W. DICKINSON, I. E. FRANKLIN and A. ability varies as a function of steel STANYA are with the Research Center, appears. chemistry, and an improved under­ Republic Steel Corporation, Independence, 2. With higher current values, the standing of these material effects is Ohio 44131 maximum or peak resistance occurs 170-sl JUNE 1980 earlier during a weld. changes in these basic electrical mea­ 3. For welds produced with high surements thus confirming some ear­ currents, the resistance trace indicates lier speculations and developing new a lower value of resistance towards the insight. completion of weld time. 3. Characterize the dynamic electri­ 4. A splash weld (expulsion), caused cal measurements over the range of by excessive welding current, is char­ weld parameters giving acceptable acterized by a sudden step in the spot welds (i.e., over the lobe curve NO EXPULSION resistance trace. area) as a first step to using these Savage6 has attempted to explain the electrical measurements for control of shape of the resistance curve on theo­ the spot welding process. retical grounds. When analyzing the WELD TIME, CYCLES resistance after each half cycle of cur­ Fig. 1— Schematic representation of dy­ Materials rent, he noted rectification which is namic electrical parameters during spot believed to indicate the presence of welding of mild steel' The spot weldability of several heats oxide films for times as long as 6 to 8 of plain carbon and high strength hot cycles on some welds. He has also rolled and cold rolled steels was inves­ attributed the rise in resistance after •. • . " :• • tigated. Specific chemical composi­ the initial few cycles to be the result of ' • ' -: •:•' ' ' tions of the materials for this investiga­ LU a EXPULSION _l tion are listed in Table 1. These include the material heating. The latter de­ o ;:\ LEVEL >- plain carbon, rimmed, renitrogenized, crease in resistance appears to coin­ o Cb-added, Cb + V-added and Cb 4- cide with the growth of the fused UJ A^AJ -NUG zone. The sudden drop in resistance 2 Mn-added steels. Also, some welds were made on a Type 304 stainless upon expulsion was attributed to the o _i SMALL OR \ steel. increase effective contact area pro­ LU BRITTLE NUGGETS'fe- vided by the expelled metal trapped Except where specifically noted, between the sheets. V: III.•^-^yk most of the data discussed are related These observations lay a pathway for to the welding of a 0.032 in. (0.8 mm) RMS SECONDARY CURRENT, AMPS effective utilization of dynamic elec­ thick plain carbon aluminum-killed trical measurements in monitoring and Fig. 2—Typical spot weld lobe curve material (material A in Table 1). control of spot welding. However, before such control can be utilized, a Equipment characterization of these electrical hibit brittleness during tearing and are All welding was performed on two measurements throughout the entire likewise considered unacceptable. Taylor-Winfield air-operated electric range of acceptable spot weld parame­ Only welds made with weld currents resistance spot welding machines. ters must be made. and times lying within the lobe area are acceptable. These are equipped with Weldtronic One method for determining the Once the lobe curve is known, char­ controllers for electronic phase con­ range over which acceptable spot trol (heat adjustment) and Duffers cur­ welds are obtained on plain carbon acterization of the dynamic electrical measurement can be made at critical rent analyzers for simultaneous mea­ sheet is through the use of spot weld surements of weld time and secondary lobe curves. A typical spot weld lobe areas on the curve. Such critical areas are a) around the lower limit line, b) at RMS weld currents. Electrode forces curve is presented in Fig. 2. A lobe expulsion, and c) within the accept­ were accurately set at the recom­ curve is a graphical representation of 7 able region. mended force for the sheet thickness ranges of welding variables over which being welded and checked several acceptable spot welds are formed on a times throughout the welding program specific material welded with a prese­ Investigation Procedure using a universal force gauge. lected electrode force. The lobe curve Objective is determined by making spot welds Electronic Circuits for Monitoring The objectives of this investigation using different weld time/weld cur­ the Dynamic Electrical Parameters rent combinations. Welds made with were to: currents and/or times exceeding the 1. Build a spot weld monitoring sys­ A schematic of the circuits used to upper curve experience expulsion on tem capable of measuring dynamic develop the welding parameters is welding and are, therefore, considered values of voltage, current, resistance, shown in Fig. 3. unacceptable. Welds made with cur­ and power. The instantaneous voltage across rents or times below the lower curve 2. Relate the phenomena occurring the electrodes is sensed by
Recommended publications
  • Effect of Corrosion Protection Method on Properties of RSW and RFSSW Lap Joints Applied in Production of Thin-Walled Aerostructu
    materials Article Effect of Corrosion Protection Method on Properties of RSW and RFSSW Lap Joints Applied in Production of Thin-Walled Aerostructures Agata Dudek 1 , Jacek Andres 2,*, Agata Wro ´nska 2 and Waldemar Łogin 2 1 Department of Production Engineering and Materials Technology, Czestochowa University of Technology, 42-218 Czestochowa, Poland; [email protected] 2 Polskie Zakłady Lotnicze Sp. z o.o.A Lockheed Martin Company, 39-300 Mielec, Poland; [email protected] (A.W.); [email protected] (W.Ł.) * Correspondence: [email protected] Received: 2 March 2020; Accepted: 8 April 2020; Published: 14 April 2020 Abstract: Aluminum structures, and in particular an element of aerostructures, are strongly exposed to the effects of weather conditions. In the case of using new techniques of joining these structural elements, the selection of proper corrosion protection without losing the required properties of the joint may determine its potential application. This paper presents the results of experimental research concerning the influence of corrosion protection on the microstructure and mechanical strength of resistance spot welded (RSW) and refill friction stir spot welded (RFSSW) joints. The tests were carried out on 2024 T3 aluminum alloy, both sides alcladed. For comparison purposes, the following joints were welded: without any protection, with the primer layer, with anodic oxide coating, and with anodic oxide coating plus sealant between the overlapping surface of the welded metal sheet. The samples were visually inspected, and metallographic and mechanical strength examination was conducted. The test results indicate that the application of the protective layers and its type have an impact on the strength of RSW and RFSSW joints.
    [Show full text]
  • Electrode Geometry Resistance Spot Welding
    A WELDING RESEARCH SUPPLEMENT TO THE WELDING JOURNAL, FEBRUARY 1990 Sponsored by the American Welding Society and the Welding Research Council - - All papers published in the Welding Journal's Welding Research Supplement undergo Peer Review before publication for: 1) originality of the contribution; 2) technical value to the welding community; 3) prior publication of the material being reviewed; 4) proper credit to others working in the same area; and 5) justification of the conclusions, based on the work performed. The names of the more than 170 individuals serving on the AWS Peer Review Panel are published periodically. All are experts in specific technical areas, and all are volunteers in the program. Electrode Geometry Resistance Spot Welding Ma thema tical model predicts current distribution as a function of electrode geometry BY R. J. BOWERS, C. D. SORENSEN AND T. W. EAGAR ABSTRACT. The effect of electrode ge- tance to the industry is the resistance The roles of welding parameters such as ometry on current distribution has been welding of various galvanized sheet steel upslope, preheat and weld time also have investigated. A mathematical mode! was products, which have become established been analyzed to determine their effects developed to evaluate current distribu- for use in automotive manufacture due to on weldability. Aspects of the electrode tion in both truncated cone (TC) and pim- their corrosion resistance. However, this itself, such as material (Ref. 1) and geom- ple-tipped (PT) electrodes. Electrode life increased corrosion protection is offset by etry (Ref. 2), have been studied as well. and lobe curve tests were conducted to the increased difficulty of welding galva- Friedman and McCauley (Ref.
    [Show full text]
  • Boilermaking Manual. INSTITUTION British Columbia Dept
    DOCUMENT RESUME ED 246 301 CE 039 364 TITLE Boilermaking Manual. INSTITUTION British Columbia Dept. of Education, Victoria. REPORT NO ISBN-0-7718-8254-8. PUB DATE [82] NOTE 381p.; Developed in cooperation with the 1pprenticeship Training Programs Branch, Ministry of Labour. Photographs may not reproduce well. AVAILABLE FROMPublication Services Branch, Ministry of Education, 878 Viewfield Road, Victoria, BC V9A 4V1 ($10.00). PUB TYPE Guides Classroom Use - Materials (For Learner) (OW EARS PRICE MFOI Plus Postage. PC Not Available from EARS. DESCRIPTORS Apprenticeships; Blue Collar Occupations; Blueprints; *Construction (Process); Construction Materials; Drafting; Foreign Countries; Hand Tools; Industrial Personnel; *Industrial Training; Inplant Programs; Machine Tools; Mathematical Applications; *Mechanical Skills; Metal Industry; Metals; Metal Working; *On the Job Training; Postsecondary Education; Power Technology; Quality Control; Safety; *Sheet Metal Work; Skilled Occupations; Skilled Workers; Trade and Industrial Education; Trainees; Welding IDENTIFIERS *Boilermakers; *Boilers; British Columbia ABSTRACT This manual is intended (I) to provide an information resource to supplement the formal training program for boilermaker apprentices; (2) to assist the journeyworker to build on present knowledge to increase expertise and qualify for formal accreditation in the boilermaking trade; and (3) to serve as an on-the-job reference with sound, up-to-date guidelines for all aspects of the trade. The manual is organized into 13 chapters that cover the following topics: safety; boilermaker tools; mathematics; material, blueprint reading and sketching; layout; boilershop fabrication; rigging and erection; welding; quality control and inspection; boilers; dust collection systems; tanks and stacks; and hydro-electric power development. Each chapter contains an introduction and information about the topic, illustrated with charts, line drawings, and photographs.
    [Show full text]
  • 1. Exposure Data
    1. EXPOSURE DATA 1.1 Description of major welding are used as part of the welding process (e.g. the processes and materials shielding gas) (ISO, 2009). While there are many welding processes Welding is a broad term for the process routinely employed in occupational settings, the of joining metals through coalescence (AWS, most common arc welding processes are manual 2010). Welding techniques tend to be broadly metal arc (MMA, ISO No. 111), gas metal arc classified as arc welding or gas welding. Arc (GMA, ISO No. 13), flux-cored arc (FCA, ISO Nos welding uses electricity to generate an arc, 114 and 136), gas tungsten arc (GTA, ISO No. 14), whereas gas or oxyfuel welding (ISO 4063:2009 and submerged arc (SA, ISO No. 12) (Table 1.2 process numbers 3, 31, 311, 312, and 313) uses fuel and Table 1.3). Electric resistance welding (ER, gases such as acetylene or hydrogen to generate ISO Nos 21 and 22) is also commonly used for spot heat. Welding results in concurrent exposures or seam welding, and uses electric currents and including welding fumes, gases, and ionizing force to generate heat. In occupational settings, and non-ionizing radiation, and coexposures these processes are most commonly used to weld from other sources such as asbestos and solvents mild steel (MS, low carbon) or stainless steel (SS). (Table 1.1). Flame cutting (ISO No. 81), the process of using Welding fumes are produced when metals oxygen (O) and a fuel to cut a metal, is a closely are heated above their melting point, vapourize related process that is often grouped occupation- and condense into fumes.
    [Show full text]
  • Effects of Refill Friction Stir Spot Weld Spacing and Edge Margin on Mechanical Properties of Multi-Spot-Welded Panels
    Journal of Manufacturing and Materials Processing Article Effects of Refill Friction Stir Spot Weld Spacing and Edge Margin on Mechanical Properties of Multi-Spot-Welded Panels Guruvignesh Lakshmi Balasubramaniam 1, Enkhsaikhan Boldsaikhan 1,* , Shintaro Fukada 2, Mitsuo Fujimoto 2 and Kenichi Kamimuki 3 1 Industrial, Systems & Manufacturing Engineering Department, Wichita State University, Wichita, KS 67260, USA; [email protected] 2 Corporate Technology Division, Kawasaki Heavy Industries, Ltd., Akashi, Hyogo 673-8666, Japan; [email protected] (S.F.); [email protected] (M.F.) 3 Aerospace Division, Kawasaki Heavy Industries, Ltd., Kakamigahara, Gifu 504-8710, Japan; [email protected] * Correspondence: [email protected]; Tel.: +1-316-978-6323 Received: 30 April 2020; Accepted: 2 June 2020; Published: 7 June 2020 Abstract: Refill friction stir spot welding (RFSSW) is an emerging technology for joining aerospace aluminum alloys. The aim of the study is to investigate the effects of the refill friction stir spot weld spacing and the edge margin on the mechanical properties of multi-spot-welded AA7075-T6 panels. AA7075-T6 is a baseline aerospace aluminum alloy used in aircraft structures. The study employs an innovative robotic RFSSW system that is designed and developed by Kawasaki Heavy Industries (KHI). The experimental strategy uses Design of Experiments (DoE) to characterize the failure loads of multi-spot-welded panels in terms of the spot weld spacing, edge margin, and heat-affected zone (HAZ) of the spot weld. The RFSSW process leaves behind a thermal “imprint” as HAZ in heat-treatable aluminum alloys. According to the DoE results, larger spot weld spacings with no HAZ overlap produce higher failure loads of multi-spot-welded panels.
    [Show full text]
  • Owen Submachine Gun.Nomination
    Nomination of OWEN SUBMACHINE GUN for an Engineering Heritage National Marker Owen Gun Mark 1/42 - skeleton stock, cooling fins on barrel source gunshows.com.nz Owen Gun Mark 1/43 - wooden stock, camouflage finish by Doug Boleyn Engineering Heritage Sydney January 2017 Table of Contents Page 1. Introduction 2 2. Nomination Letter 4 3. Nomination Support Information Basic Data 5 4. Basic History 8 5. Engineering Heritage Assessment 11 6. Interpretation Plan 14 7. References & Acknowledgements 15 Appendices 1. Statement of Support for Engineering Heritage Recognition 16 2. History Time Line of the Owen Submachine Gun 17 3. Photos of the Owen Submachine Gun and other submachine guns used 28 in World War 2 4. Drawings of the Owen Submachine Gun 34 5. Statistics of the various models of the Owen Gun and Comparison Table 35 6. Biographies of Companies and People Associated with the Owen Gun 39 7. Glossary Terminology and Imperial Unit Conversions 44 8. Author's Assessment of Engineering Heritage Significance Check List 45 Rev 05 01 17 Page 1 1. Introduction. The Owen submachine gun [SMG] (1) that bears its designer's name was the only weapon of World War 2 used by Australian troops that was wholly designed and manufactured in Australia. Conceptually designed by Evelyn Owen, a committed young inventor, the concept was further developed to production stage by Gerard Wardell Chief Engineer Lysaght's Newcastle Works Pty Limited - Port Kembla Branch (2) [Lysaghts] with the assistance of Evelyn Owen ( and Fred Kunzler a Lysaght employee who had been a gunsmith in his native Switzerland.
    [Show full text]
  • Crackin G in Spot Welding Aluminum Alloy AA5754 Cracking and Its Mechanisms During the Resistance Spot Welding of Aluminum Alloys Are Analyzed
    Crackin g in Spot Welding Aluminum Alloy AA5754 Cracking and its mechanisms during the resistance spot welding of aluminum alloys are analyzed BY J. SENKARA AND H. ZHANG ABSTRACT. The phenomenon of crack- technique in auto-body assembly, resis- during spot welding. Toyota reported so- ing was observed during resistance spot tance spot welding is used for joining alu- lidification failure in the nugget or liqua- welding a commercial aluminum alloy minum parts, as it has been used for steel. tion cracking in the heat-affected zone AA5754, and mechanisms of cracking The nonheat-treatable AI-Mg alloys (HAZ) for one of the 5000 series alloys and healing are discussed in this paper. (5000 series) in sheet product form are containing above 5 wt-% Mg (Ref. 13). Metallographic study of welded coupons among the most promising aluminum They observed cracking under a wide revealed cracks located on only one side materials, and among them, AA5754 has range of welding parameters and sug- of a weldment in the heat-affected zone been developed especially for the auto- gested that preheating or increasing (HAZ), with respect to the welding se- motive industry. The optimized magne- welding time may decrease thermal quence. Cracks are visible from longitu- sium content in the alloy assures satis- stresses and therefore decrease cracking dinal cross sections only. Some of them factory mechanical properties and low tendency. The possibility of cracking was are partially or fully filled. Crack appear- susceptibility to stress corrosion crack- also indirectly implicated in spot welding ance and orientation are fairly repeatable ing. The AA5754 alloy has good forma- AA5754 by Thornton, et al.
    [Show full text]
  • Effects of Welding on Health
    Effects of Welding on Health, XII Key Words—Welding, health, cancer, disease, exposure, fumes, gases, literature review, metal fume fever, noise, radiation, toxicology Effects of Welding on Health, XII Prepared for AWS Safety and Health Committee Research performed by Biomedical Toxicology Associates Frederick, Maryland Written by Winifred G. Palmer, Ph.D. and James C. Eaton, P.E. Abstract This literature review, with 216 citations, was prepared under contract to the American Welding Society for its Safety and Health Committee. The review deals with studies of the fumes, gases, radiation, and noise generated during various welding processes. Section 1 summarizes recent studies of occupational exposures, Section 2 contains information related to the human health effects, and Section 3 discusses the effects of welding on animals and cell cultures. 550 N.W. LeJeune Road, Miami, Florida 33126 This page is intentionally blank. International Standard Book Number: 0-87171-724-7 American Welding Society, 550 N.W. LeJeune Road, Miami, FL 33126 © 2003 by American Welding Society. All rights reserved Printed in the United States of America This report is published as a service and convenience to the welding industry and is the product of an independent con- tractor (Biomedical Toxicology Associates) which is solely responsible for its contents. The materials in this report have not been independently reviewed or verified and are offered only as information. AWS assumes no responsibility for any claim that may arise from the use of this information. Users should make independent investigations to determine the appli- cability of this information for their purposes. Personnel AWS Safety and Health Committee S.
    [Show full text]
  • Award No. 1529 Docket No. 1387 2-MP-CM-'52
    Award No. 1529 Docket No. 1387 2-MP-CM-‘52 NATIONAL RAILROAD ADJUSTMENT BOARD SECOND DIVISION The Second Division consisted of the regular members and in addition Referee Jay S. Parker when award was rendered. PARTIES TO DISPUTE: SYSTEM FEDERATION NO. 2, RAILWAY EMPLOYES’ DEPARTMENT, A. F. of L. (Carmen) MISSOURI PACIFIC RAILROAD COMPANY DISPUTE: CLAIM OF EMPLOYES: (a) That carrier is violating the controlling agreement at North Little Rock Shops, particularly Rules 29 and 136 (a) by refusing to pay the welders’ rate of pay to Car-man Welder R. A. Parkhill when assigned to operating spot welding machine. (b) In consideration of the foregoing, Carman Welder R. A. Parkhill is entitled to be additionally compensated in the amount of 5c per hour from March 21, 1949 to August 31, 1949, both dates inclusive, and 6c per hour from September 1, 1949, to date, for all time engaged in operating spot welding machine. EMPLOYES’ STATEMENT OF FACTS: At North Little Rock, carrier maintains a universal or multirange spot welder in coach shop. This machine is presently operated by Carman R. A. Parkhill, hereinafter referred to as the claimant, and is capable of welding all types and gauges of metal from 28% to 1/2 inch, inclusive. When machine was first installed, a factory representative was on hand to teach claimant how to operate machine, which was a slow process at first because in addition to learning the actual operation, he had to acquire a thorough knowledge of the various metals and their reaction to the spot welding process in order to set the electronic controls for maximum weld- ing efficiency.
    [Show full text]
  • What Is Welding?
    What is welding? The first step toward achieving welding safety is to mission apparatus with clutches, gears and cou- follow the safety and maintenance instructions sup- plings should have these danger points screened plied by the manufacturer of the apparatus. or guarded. Insulate all parts that carry current. Turn off the generator before changing electrodes Next, the welder should check the equipment. or cables. Have a compentent person condust a thorough inspection of all equipment at least once a month. If using a gasoline-powered generator indoors or Replace or repair excessively worn equipment. Dis- in a confined space, transmit the exhaust outdoors continue using unsafe or defective equipment until to prevent an accumulation of carbon monoxide. you make repairs. Use replacement parts specified Also, check for fuel leaks. by the equipment’s manufacturer. Keep machines clean. To prevent excessive flash- Safety-approved electrical arc welding equipment ing, keep commentators clean; for cleaning, use should meet the standards of the National Electri- No. 00 sandpaper, not flammable liquids. Keep rec- cal Manufacturers Association (NEMA). Most insur- tifiers free of dust or lint that could interfere with ance companies and local authorities recognize ventilation. oxygen and acetylene equipment listed by Under- writers’ Laboratories Inc. Check the cables While the safety suggestions in this booklet apply Welding cables should have high-quality insula- specifically to portable welding equipment and its tion, and should be flexible and large enough for use, they also are generally applicable for the safety the job. Overloading burns away the insulation, maintenance and operation of stationary welding causing both shock and fire hazards.
    [Show full text]
  • Friction Stir Spot Welding of Aluminum and Copper: a Review
    materials Review Friction Stir Spot Welding of Aluminum and Copper: A Review 1,2, 1, , 3,4 5,6 1,7 Mingshen Li y , Chaoqun Zhang * y, Dayong Wang , Li Zhou , Daniel Wellmann and Yingtao Tian 7 1 Shanghai Key Laboratory of Digital Manufacture for Thin-Walled Structures, School of Mechanical Engineering, Shanghai Jiao Tong University, Shanghai 200240, China; [email protected] (M.L.); [email protected] (D.W.) 2 School of aerospace engineering, Shenyang Aerospace University, Shenyang 110136, China 3 State Key Laboratory of Long-Life High Temperature Materials, Dong Fang Turbine Co., Ltd. Deyang Sichuan 61800, China; [email protected] 4 Dongfang Electric Corporation Dongfang Turbine Co., LTD, Deyang 618000, China 5 State Key Laboratory of Advanced Welding and Joining, Harbin Institute of Technology, Harbin 150001, China; [email protected] 6 Shandong Provincial Key Laboratory of Special Welding Technology, Harbin Institute of Technology at Weihai, Weihai 264209, China 7 Department of Engineering, Lancaster University, Bailrigg, Lancaster LA1 4YW, UK; [email protected] * Correspondence: [email protected] or [email protected]; Tel.: +86-21-34206543 M.L. and C.Z. contribute equally to this paper. y Received: 16 November 2019; Accepted: 26 December 2019; Published: 31 December 2019 Abstract: Aluminum (Al) and copper (Cu) have been widely used in many industrial fields thanks to their good plasticity, high thermal conductivity and excellent electrical conductivity. An effective joining of dissimilar Al and Cu materials can make full use of the special characteristics of these two metals. Friction stir spot welding (FSSW), as an efficient solid-state welding method suitable for joining of dissimilar metal materials, has great prospects in future industrial applications.
    [Show full text]
  • Weldability and Degradation Study of Coated Electrodes for Resistance Spot Welding
    Weldability and Degradation Study of Coated Electrodes for Resistance Spot Welding By Kevin Randall Chan A thesis presented to the University of Waterloo in fulfillment of the thesis requirement for the degree of Master of Applied Science in Mechanical Engineering Waterloo, Ontario, Canada © Kevin Randall Chan, 2005 I hereby declare that I am the sole author of this thesis. I authorize the University of Waterloo to lend this thesis to other institutions or individuals for the purpose of scholarly research. Kevin R. Chan I further authorize the University of Waterloo to reproduce the thesis by photocopying or other means, in total or in part, at the request of other institutions or individuals for the purpose of scholarly research. Kevin R. Chan ii The University of Waterloo requires the signatures of all persons using or photocopying this thesis. Please sign below, and give address and date. iii Abstract In resistance spot welding of hot dipped galvanized steel sheet, the effect of a TiC metal matrix composite coated electrode on weldability, electrode life and degradation processes was studied. A review of the resistance spot welding process is given, followed by a literature study of the known issues when welding zinc coated steels and some of the methods explored to address those issues. Coated and uncoated Class II CuCrZr domed-flat ‘B’ nose electrodes were used to conduct welding trials. To study the weldability of the coated electrodes compared to the uncoated electrodes, both types were subjected to increasing weld current and time while monitoring resultant weld size. Overall, the coated electrodes showed an improved weldability over the uncoated electrode.
    [Show full text]