Intergranular Attack in Welded Stress-Corrosion Resistant Stainless Steels

Total Page:16

File Type:pdf, Size:1020Kb

Load more

Intergranular Attack in Welded Stress-Corrosion Resistant Stainless Steels Satisfactory stress corrosion resistance is obtained using arc welding and, depending on the base metal, Type 376/. or 309L stainless steel filler metals BY J. HONEYCOMBE AND T. C. GOOCH Introduction approaches to avoiding chloride- examined metallographically. induced SCC. The materials were a Although austenitic stainless steels conventional ferritic grade (AISI 430) SMA Welds have excellent corrosion resistance in to afford a base-line for comparison, a All the manual metal arc welds a wide variety of media, they exhibit a ferrite-martensite alloy, two ferrite- employed a 75 deg included angle, high susceptibility to stress corrosion austenite steels, and a fully ferritic single V-groove preparation with a 1.5 cracking (SCC) in hot aqueous envi­ steel having extra low interstitial (ELI) mm (0.060 in.) root face and no root ronments containing chloride or hy- element content.* The particular ma­ gap, and were made with an autoge­ droxyl ions. Industrial interest has, terials employed and the available nous GTA root and argon back purging therefore, been increasing in ferritic thicknesses are given in Table 1. and duplex-structured stainless steels for better control of penetration. The welds in the ferritic-austenitic (containing 17-27% chromium with Test Weld Preparation 0-5%Ni) which are resistant to stress alloys were deposited using nomi­ corrosion cracking. Despite their The processes employed were nally high and low energy inputs.t resistance to SCC, the conventional shielded metal arc (SMA), gas tungsten With the single phase 26%Cr-1%Mo, ferritic stainless steels containing arc (GTA), gas metal arc (GMA), because of its tendency to grain about 17%Cr possess several disadvan­ submerged arc (SA) and electron beam growth, low energy inputs only were tages; in particular, their welded joints (EB). Apart from the autogenous GTA used. may show excessive grain growth and and EB welds, three types of commer­ embrittlement, and sensitivity to inter­ cially available filler metals were GTA Welds granular corrosion.' selected for study—a matching or near- Joint preparation and root run were matching alloy; an austenitic stainless Alloys have been recently devel­ as used with the SMA welds. For the steel (either 18/10/3Mo or 23/12/Mo, oped in an attempt to overcome these 26%Cr-1%Mo steel, the argon gas flow subsequently referred to as Types 316L problems. In view of the wide range of through the torch was kept high at potential applications of such alloys, or 309L-Mo respectively) as might be employed in practice;- and a nickel approximately 25-30 l/min with back an investigation was initiated at The purging maintained at 6 l/min;1 for the Welding Institute to study their weld­ alloy, as in principle representing a weld metal of high resistance to chlo­ other steels, the torch flow rate was 10 ing behavior so that practical recom­ l/min. mendations regarding optimum pro­ ride-induced stress corrosion. The cedures can be formulated. The pres­ nominal compositions of the filler metals used are shown in Tables 2 and ent paper considers the effects of GMA Welds welding in causing susceptibility to 3, with available deposit analyses. The preparation used was a 70 deg intercrystalline attack of representa­ Butt welds were made in a restrain­ single V-groove with a 3 mm (0.12 in.) tive materials. ing jig as indicated in Tables 4 and 5, root face and no root gap. Following with interpass temperature being held welding from one side, the weld was at 150 C (302 F) maximum. No weld Materials back gouged and a sealing run inserted was given a postweld heat treatment. on the reverse side. The alloys studied were intended to Transverse sections of all welds were The shielding gas for the two duplex cover the different microstructural alloys was argon-2%0L. or argon *Material was tested as 2.5 mm (0.1 in.) depending on the filler, while for the Paper presented at the 58th AWS Annual thick sheet and 13 mm (0.5 in.) plate. It is 26%Cr-1%Mo it was either pure argon Meeting held in Philadelphia, Pennsylvania, understood from the material manufacturer or argon-1%0,. The gas flow was kept during April 25-29, 1977. that subsequent to carrying out the present high with argon back purging in all tests on the thinner material, the composi­ j. HONEYCOMBE is Senior Research Met­ tion has been modified, although no details allurgist and T. C. COOCH is Principal are available. The thicker material was Research Metallurgist, The Welding Insti­ supplied and tested after the reported jEncrgy input defined as: (Volts X Amps tute, Abington, Cambridge, England. composition change. X 60/speed (mm/min) X 1000) x kj/mm WELDING RESEARCH SUPPLEMENT I 339-s Table 1-Analyses of Steels Studied, Wt-% Material Sample thickness, mm C Mn Si S P Ni Cr Mo Nb Ti Cu O N Steel 1: 17%Cr 2.5 0.083 0.33 0.34 0.009 0.029 0.23 16.44 0.08 0.005 <0.01 0.08 0.006 0.034 Steel 2: 16%Cr-2.5%Ni- 1%Mo 2 0.035 0.66 0.47 0.006 0.009 2.72 15.91 1.22 0.5 <0.01 0.03 0.006 0.028 Steel 3: 26%Cr-1%Mo 2.6 0.007 <0.01 0.23 0.009 0.01 0.12 25.8 0.99 0.005 <0.01 <0.01 0.002 0.012 13 0.003 <0.05 0.35 0.009 0.01 0.15 26.2 0.99 0.06 <0.05 <0.05 0.002 0.012 Steel 4: 26%Cr-5%Ni- 1.5%Mo 10 0.026 0.74 0.63 0.006 0.02 5.15 26.25 1.3 0.05 <0.05 <0.05 0.005 0.07 Steel 5: 18%Cr-5%Ni- <0.05 2.5%Mo 13 0.025 1.66 1.69 0.010 0.02 5.2 18.7 2.78 <0.05 <0.05 0.003 0.07 Table 2-Nominal Analyses of Filler Metals, Wt-% Filler metal C Cr Mo Ti Si Mn Ni Nb S P Fe Cu N Matching steel 3 bare <0.005 27.5 0.99 - 0.22 0.02 0.06 - 0.014 0.010 Bal 0.02 <0.012 electrode Matching steel 4 0.10 26.0 1.50 — 0.50 1.50 5.0 - 0.015 0.015 Bal covered electrode 0.05 25.5 2.0 0.5 1.4 6.5 Type 316L covered 0.03 19.0 3.0 - 0.25 1.3 12.5 - 0.02 0.03 Bal electrode max Type 309L-Mo covered 0.03 23 2.5 - 0.8 2.5 12 - 0.03 0.04 Bal electrode Ni-base covered 0.1 13- 0.5- - 0.75 2 Bal 1.0- 0.02 — 6.12 electrode max 17 2.5 max 3.0 max Near matching steel 4 0.06 25 2 - 1.0 1.0 5 - - - Bal bare electrode Type 316L bare 0.025 18.5 2.7 - 0.85 1.35 11.5 - 0.015 0.015 Bal electrode Ni-base bare electrode 0.030 20 0.3 0.2 3.0 72 2.5 0.010 0.010 1.0 max max max max cases. Welding was mechanized, and preference to other comparable im­ The remaining two coupons were the top of each run was ground to mersion tests, such as the acid ferric suspended for 72 h in boiling acidified remove any oxide contamination. sulphate procedure, on the basis of its copper sulphate; on removal one was generally satisfactory history of prac­ bent as for the control specimen. From SA Welds tical application for other than highly the second, a section was taken trans­ oxidizing media. Another reason was verse to the weld, mounted and Incoflux 6, dried for 2 h at 200 C (392 its common use in the UK for quality polished. The depth of penetration of F) was used for all welds. Joint prepa­ control of stainless steel products. any grain boundary attack was mea­ ration was as for the GMA welds. The potentiostatic technique was sured at X400 magnification."' Welding on the first side was com­ employed because, in principle, it In addition, selected welds were pleted, the root run removed and a gives information relevant to a range exposed to the "modified" acid cop­ sealing run deposited. of environmental conditions and has per sulphate test electrolyte with been successfully used to define copper turnings in the test flask." EB Welds conditions causing intercrystalline at­ Susceptibility to intergranular attack The EB welds were made with a tack in austenitic materials.' was assessed by depth of penetration square butt preparation and no filler measurements. metal. Strauss Testing Potentiostatic Studies Strauss tests were conducted on all Corrosion Testing welds according to BS 1449: Part 4: In the first instance, potentiostat 1967. Three coupons were removed scans were conducted on all base General Comments transversely to the welds, as in Fig. 1, metals under investigation. Specimens A number of different test methods and the sides abraded to a 600 emery with 1 cm2 surface area were mounted have been developed to assess suscep­ finish. and polished to a 1,um finish. The basic tibility to intercrystalline attack in One coupon was used as a control electrolyte used was a 20% H,SO, stainless steels. When selecting evalu­ sample to allow for any difficulty in containing O.lg/I NH..CNS and the ation techniques, it is necessary that interpreting results of the necessary applied voltage was changed at 0.3 the data obtained should be relevant bend tests due to sample brittleness.
Recommended publications
  • Intergranular Corrosion (IGC)

    Intergranular Corrosion (IGC)

    Intergranular Corrosion (IGC) Example: Weld Decay When stainless steel (SS) is Microstructure of metals and alloys is made up of grains (separa ted by heated to about 650 0C, Cr C grain boundaries) 23 6 carbides form at the GB and the metal is said to be “sensitised ” Intergranular corrosion is a localized attack along the grain bo undaries, or immediately adjacent to grain boundaries, while the bulk of t he Cr -rich GB precipitates lead to a grains remain largely unaffected local depletion of Cr immediately Cr C adjacent to these precipitates, IGC is associated: 23 6 leaving these areas vulnerable to 1. With chemical segregation effects (impurities segregate at grain corrosive attack in certain boundaries) electrolytes. 2. Precipitate of compounds (e.g; carbides) at grain boundaries If the Cr concentration falls low IGC then occurs at the GB phase that has lost an element necessa ry enough (<9%), SS will no longer for adequate corrosion resistance: the GB becomes more anodic remain passive and corrosion relative to the rest of the metal surface (which is cathodic). occurs. Sensitisation of SS “Sensitisation ” of stainless Prevention of weld decay: steels is also common in the heat affected zone (HAZ) during welding and the resultant 1. Use low carbon content grade stainless steel, e.g: 316L, 304L ~ corrosion is known as “weld 0.03 wt%, so carbide formation is minimal. IGC in HAZ of SS decay ” 2. Use a stabilised grade of SS, which contain strong carbide -forming Many Al base alloys are elements such as Nb or Ti susceptible to IGC if phases present at GB ’s are anodic to Al 3.
  • Intergranular Corrosion of Extruded Alloy AA6005 and AA6082

    Intergranular Corrosion of Extruded Alloy AA6005 and AA6082

    Proceedings of the 9th International Conference on Aluminium Alloys (2004) 818 Edited by J.F. Nie, A.J. Morton and B.C. Muddle © Institute of Materials Engineering Australasia Ltd Intergranular Corrosion of Extruded AA6000-Series Model Alloys G. Svenningsen1, M. Hurlen Larsen1, J-E. Lein2, J-H. Nordlien3, K. Nisancioglu1 1 Department of Materials Technology, NTNU, NO-7491 Trondheim, Norway 2 SINTEF Materials Technology, NO-7465 Trondheim, Norway 3 Hydro Aluminium, R&D Materials Technology, NO-4265 Håvik, Norway Keywords: AlMgSi alloys, intergranular corrosion, Q-phase Abstract Susceptibility to intergranular corrosion (IGC) of 6000-series model alloys extruded in the laboratory was investigated as a function of Cu content, cooling rate after extrusion and artificial aging. One alloy type contained about 0.6 wt% each of Mg and Si with varying Cu content. The second type was a Cu-free alloy with higher Si content (ca. 1%). Extrusions with low Cu content (≤ 0.02 wt%) were resistant to localised corrosion, while those with high Cu content (0.17 wt%) could become susceptible to IGC. FE-SEM investigation revealed large grain boundary precipitates on air cooled samples. These precipitates were Mg2Si and Q-phase (Al5Cu2Mg8Si6) in the samples susceptible to IGC. Only Mg2Si was present in the corrosion-resistant samples. IGC susceptibility was attributed to the microgalvanic coupling between the noble Q-phase particles and the adjacent depleted zone. IGC can be prevented by proper heat treatment. 1. Introduction IGC is the result of microgalvanic processes along grain boundaries [1,2]. Galvanic coupling between the grain boundary particles and the matrix, grain boundary particles and the adjacent depleted zone, or between matrix and the depleted zone may result in preferential corrosion along the grain boundary.
  • High-Performance Alloys for Resistance to Aqueous Corrosion

    High-Performance Alloys for Resistance to Aqueous Corrosion

    High-Performance Alloys for Resistance to Aqueous Corrosion Wrought nickel products The INCONEL® Ni-Cr, Ni-Cr-Fe & Ni-Cr-Mo Alloys The INCOLOY® Fe-Ni-Cr Alloys The MONEL® Ni-Cu Alloys 63 Contents Corrosion Problems and Alloy Solutions 1 Corrosion-Resistant Alloys from the Special Metals Group of Companies 4 Alloy Selection for Corrosive Environments 11 Corrosion by Acids 12 Sulfuric Acid 12 Hydrochloric Acid 17 Hydrofluoric Acid 20 Phosphoric Acid 22 Nitric Acid 25 Organic Acids 26 Corrosion by Alkalies 28 Corrosion by Salts 31 Atmospheric Corrosion 35 Corrosion by Waters 37 Fresh and Process Waters 37 Seawater and Marine Environments 38 Corrosion by Halogens and Halogen Compounds 40 Fluorine and Hydrogen Fluoride 40 Chlorine at Ambient Temperature 41 Chlorine and Hydrogen Chloride at High Temperatures 41 Metallurgical Considerations 44 Appendix 49 Corrosion Science and Electrochemistry 50 References 60 Publication number SMC-026 Copyright © Special Metals Corporation, 2000 INCONEL, INCOLOY, MONEL, INCO-WELD, DURANICKEL, 625LCF, 686CPT, 725, 864 and 925 are trademarks of the Special Metals group of companies. Special Metals Corporation www.specialmetals.com Corrosion Problems and Alloy Solutions Due to their excellent corrosion resistance and good mechanical properties, the Special Metals nickel-based alloys are used for a broad range of applications in an equally broad range of industries, including chemical and petrochemical processing, pollution control, oil and gas extraction, marine engineering, power generation, and pulp and paper manufacture. The alloys' versatility and reliability make them the prime materials of choice for construction of process vessels, piping systems, pumps, valves and many other applications designed for service in aqueous and high-temperature environments.
  • Transitions Between Pitting and Intergranular Corrosion in AA2024

    Transitions Between Pitting and Intergranular Corrosion in AA2024

    Electrochimica Acta, 2003, Volume 48, Issue 9, Pages 1193-1210. ISSN: 0013-4686 DOI: 10.1016/S0013-4686(02)00828-9 © 2003 Elsevier Science Ltd. All rights reserved. http://www.sciencedirect.com/science/article/B6TG0-47TWXK6-5/2/6578b9e305630eb8703b80b216e7e58f http://www.elsevier.com/wps/find/journaldescription.cws_home/205/description#description Transitions between pitting and intergranular corrosion in AA2024 Weilong Zhang, G.S. Frankel Fontana Corrosion Center, Department of Materials Science and Engineering, The Ohio State University Abstract The pitting and intergranular corrosion (IGC) behavior of various tempers of AA2024 was investigated in 1 M NaCl. The breakdown potentials associated with pitting or IGC were determined. The breakdown potentials were found to be almost independent of sample orientation for any given temper. Artificial aging had a strong effect on polarization behavior and localized corrosion morphology. The anodic polarization curves of AA2024 in the solution heat treated and water-quenched condition, T3, and T3+ tempers exhibited two breakdown potentials, whereas overaged AA2024-T8, T8+ , and solutionized and furnace cooled AA2024 exhibited only one breakdown potential. When two breakdown potentials were observed, the more active one was found to be related to the transient dissolution of S phase Al2CuMg particles leading to pitting while the noble one was thought to result primarily from initiation and growth of IGC. The breakdown potentials decreased with increasing aging time at 190°C, and only one breakdown potential was measured for T8 and T8+ tempers. Unlike the T3 temper, no sharp IGC was found for these tempers. Selected granular attack from breakdown of the copper-depleted matrix was believed to be the cause for localized corrosion in the T8 and T8+ tempers.
  • Growth Opportunities & Emerging Trends in Corrosion

    Growth Opportunities & Emerging Trends in Corrosion

    Growth Opportunities & Emerging Trends in Corrosion Resistant Pipe Market Lucintel Brief Published : December 2014 Table of Contents • Executive Summary • Corrosion in Global Pipe Market • Global Pipe Market Insights • Key Corrosion Resistant Pipes • Strategic Growth Opportunities for Corrosion Resistant Pipes • About Lucintel 2 Executive Summary • Global pipe market was estimated at ~$200 billion in 2013 • Steel pipes are the most dominant in the global pipe market. Other dominant pipes are concrete and plastic pipes, especially the PVC pipes • In the global pipe industry, corrosion is a serious issue across industries such as oil and gas exploration, oil and gas transmission, industrial and chemical, sewage, marine, water and waste water, etc. • Key piping system applications include chlorine/caustics handling, water lines, vent lines, sludge and slurry lines, brine slurry, floor drains, etc. • High cost of corrosion has led to increased usage of corrosion control mechanisms such as protective coatings, corrosion resistant materials, cathodic protection, and corrosion inhibitors • Corrosion resistant pipes are gaining traction as a means of corrosion control and mitigation. • Key corrosion resistant pipes include metallic pipes made of stainless steel, carbon steel, nickel and it’s alloys, titanium and it’s alloys, etc. and non-metallic pipes made of such as fiber reinforced plastics (FRP), polypropylene (PP), fluoropolymers, etc. • Titanium and nickel pipes are most suitable in extreme conditions, but there use is limited due to high cost • PVC/CPVC, FRP, PP, and other plastics are preferred in medium temperature conditions and offer high cost benefit advantage as compared to titanium and nickel • Demand for corrosion resistant pipes is likely to surge in emerging applications such as flue gas desulfurization, hydraulic fracking, mineral extraction, etc.
  • Regulatory Guide 3.37, Guidance for Avoiding Intergranular Corrosion and Stress Corrosion in Austenitic Stainless Steel Componen

    Regulatory Guide 3.37, Guidance for Avoiding Intergranular Corrosion and Stress Corrosion in Austenitic Stainless Steel Componen

    U.S. NUCLEAR REGULATORY COMMISSION September 1975 REGU LATORY GUIDE OFFICE OF STANDARDS DEVELOPMENT REGULATORY GUIDE 3.37 GUIDANCE FOR AVOIDING INTERGRANULAR CORROSION AND STRESS CORROSION IN AUSTENITIC STAINLESS STEEL COMPONENTS OF FUEL REPROCESSING PLANTS A. INTRODUCTION are designed to allow one to detect and control (a) improperly processed or fabricated materials and (b) Section 50.34, "Contents of applications: technical conditions that could lead to intergranular corrosion and information," of 10 CFR Part 50, "Ucensing of Produc- stress corrosion cracking during fabric'n or service of tion and Utilization Facilities," requires, among other austenitic stainless steels. The recc crendations of this things, that each application for a construction permit guide apply to austenitic stainlesROLused in safetyt for a fuel reprocessing plant include sufficient informa- related process equipment wit assodW vessels and tion relative to construction materials tqyrovide reason- piping, radioactive waste d storage systems, able asrance that the final design will conform to the metal liners of proc te storage tank design 'bases with adequate margin for safety. Section vaults, and other sa -rela tructures, systems, and 50.34 also requires a discussion of how the applicable components of fue requirements of Appendix B, "Quality Assurance Cri teria for Nuclear Power Plants and Fuel Reprocessing USSiON Plants," to 10 CFR Part 50 will be satisfied. As used in Appendix B, "quality assurance" comprises D11 those e e and decontamination of radiochem planned and systematic actions necessary to provide i ce u ment,t structures, and components can adequate confidence that safety-related structures, sys- be t and hazardous. Cracks, crevices, and tems, and components will perform satisfactorily inr ies on the surfaces of radiochemical equip service.
  • The Localized Corrosion and Stress Corrosion Cracking of a 6005A-T6 Extrusion Profile

    The Localized Corrosion and Stress Corrosion Cracking of a 6005A-T6 Extrusion Profile

    materials Article The Localized Corrosion and Stress Corrosion Cracking of a 6005A-T6 Extrusion Profile Jijun Ma 1,*, Jing Sun 1, Quanmei Guan 1, Qingwei Yang 2, Jian Tang 2, Chengxiong Zou 2 , Jun Wang 2,3, Bin Tang 2,3 , Hongchao Kou 2,3, Haisheng Wang 1, Jun Gao 1, Jinshan Li 2,3,* and William Yi Wang 2,3,* 1 CRRC Tangshan Co., Ltd., Tangshan 063035, China; [email protected] (J.S.); [email protected] (Q.G.); [email protected] (H.W.); [email protected] (J.G.) 2 State Key Laboratory of Solidification Processing, School of Materials Science and Engineering, Northwestern Polytechnical University, Xi’an 710072, China; [email protected] (Q.Y.); [email protected] (J.T.); [email protected] (C.Z.); [email protected] (J.W.); [email protected] (B.T.); [email protected] (H.K.) 3 Innovation Center, NPU Chongqing, Chongqing 401135, China * Correspondence: [email protected] (J.M.); [email protected] (J.L.); [email protected] (W.Y.W.) Abstract: In the present work, the localized corrosion and stress corrosion cracking (SCC) behaviors of a commercial 6005A-T6 aluminum extrusion profile was studied comprehensively. The velocity of crack growth in self-stressed double-cantilever beam (DCB) specimens under constant displacement was estimated, which also provides insight into the local microstructure evolutions at the crack tips caused by the localized pitting corrosion, intergranular corrosion (IGC), and intergranular SCC. Characterizations of local corrosion along the cracking path for a period of exposure to 3.5% NaCl were revealed via optical microscope (OM), scanning electron microscope (SEM), and electron backscatter diffraction (EBSD).
  • Practical Guidelines for the Fabrication of Duplex Stainless Steel

    Practical Guidelines for the Fabrication of Duplex Stainless Steel

    Practical Guidelines for the Fabrication of Duplex Stainless Steels Practical Guidelines for the Fabrication of Duplex Stainless Steel Second edition 2009 © IMOA 1999-2009 ISBN 978-1-907470-00-4 Published by the International Molybdenum Association (IMOA), London, UK www.imoa.info [email protected] Prepared by TMR Stainless, Pittsburgh, PA, USA Designed by circa drei, Munich, Germany Acknowledgement: IMOA is grateful to the Inter national Stainless Steel Forum and Euro Inox for their support and review of this handbook. We would furthermore like to thank the following com panies for their detailed feed- back and contributions: Acerinox, Allegheny Ludlum, Aquatech, ArcelorMittal, Baosteel, Columbus Stainless, JSL Limited, Nippon Yakin Kogyo, North American Stainless, Outokumpu Stainless, Sandvik, Swagelok, and Yieh United Steel Corporation. The International Molybdenum Association (IMOA) has made every effort to ensure that the information presented is technically correct. However, IMOA does not represent or warrant the accuracy of the infor- mation contained in this handbook or its suitability for any general or specific use. The reader is advised that the material contained herein is for information purposes only; it is not intended as a substitute for any person’s procedures, and should not be used or relied upon for any specific or general application without first obtaining competent advice. IMOA, its members, staff and consultants specifically disclaim any and all liability or responsibility of any kind for loss, damage, or injury resulting from the use of the information contained in this publication. ASTM’s and EN international specifications were used pre- dominantly in this publication; however, material specifications may vary among countries.
  • Microstructure and Intergranular Corrosion of the Austenitic Stainless Steel 1.4970

    Microstructure and Intergranular Corrosion of the Austenitic Stainless Steel 1.4970

    Journal of Nuclear Materials 358 (2006) 40–46 www.elsevier.com/locate/jnucmat Microstructure and intergranular corrosion of the austenitic stainless steel 1.4970 Maysa Terada a, Mitiko Saiki a, Isolda Costa a,*, Angelo Fernando Padilha b a Instituto de Pesquisas Energe´ticas e Nucleares (IPEN/CNEN-SP) Av. Professor Lineu Prestes, 2242 Cidade Universita´ria, 05508-900 Sa˜o Paulo (SP), Brazil b Departamento de Engenharia Metalu´rgica e de Materiais da Universidade de S. Paulo Av. Professor Mello Moraes, 2463, 05508-030 Sa˜o Paulo (SP), Brazil Received 9 November 2005; accepted 29 June 2006 Abstract The precipitation behaviour of the DIN 1.4970 steel and its effect on the intergranular corrosion resistance were studied. Time–temperature–precipitation diagrams for the secondary phases (Ti,Mo)C, (Cr,Fe,Mo,Ni)23C6 and (Cr,Fe)2B are presented and representative samples have been selected for corrosion studies. The susceptibility to intergranular corrosion of the samples was evaluated using the double loop electrochemical potentiokinetic reactivation technique. The results showed that the solution-annealed samples and those aged at 1173 K did not present susceptibility to intergranular cor- rosion, whereas aging treatment from 873 to 1073 K resulted in small susceptibility to intergranular attack that decreased with aging temperature. The preferential formation of (Ti,Mo)C at higher aging temperatures comparatively to M23C6, retained the chromium in solid solution preventing steel sensitization and, consequently, intergranular corrosion. Ó 2006 Elsevier B.V. All rights reserved. 1. Introduction beneficial effects such as prevention of intergranular corrosion, reduction of void swelling and helium The titanium-stabilized full austenitic chromium– embrittlement, and precipitate strengthening [1].
  • Exfoliation Corrosion Kinetics of High Strength Aluminum Alloys

    Exfoliation Corrosion Kinetics of High Strength Aluminum Alloys

    EXFOLIATION CORROSION KINETICS OF HIGH STRENGTH ALUMINUM ALLOYS DISSERTATION Presented in Partial Fulfillment of the Requirements for the Degree of Doctor of Philosophy in the Graduate School of The Ohio State University By Xinyan Zhao, M.S. ***** The Ohio State University 2006 Dissertation Committee: Dr. Gerald S. Frankel, Adviser Approved by Dr. Rudolph G. Buchheit ____________________________ Dr. Michael J. Mills Adviser Dr. Stanislav I. Rokhlin Graduate Program in Materials Science and Engineering ABSTRACT The objectives of this study were to quantitatively study localized corrosion, especially exfoliation corrosion (EFC), of high strength aluminum alloys and to investigate the mechanism of exfoliation corrosion with a focus on the effects of alloy temper, microstructure, relative humidity (RH) and mechanical stress. A new technique, Exfoliation of Slices in Humidity (ESH) was developed for the determination of exfoliation corrosion (EFC) susceptibility and quantification of EFC kinetics. Two AA7178 plates taken from the wingskin of a retired KC135 airplane were used as test samples. Slices of the plate were pretreated by potentiostatic polarization in chloride solution to develop localized corrosion sites. Subsequent exposure to high humidity after pretreatment of properly oriented and unconstrained samples resulted in the development of EFC at the edges of the slices. The EFC kinetics was determined by measuring the width of the central unattacked region of the samples. The ESH results were representative of the different EFC behavior of the two plates during outdoor exposure. These results show the capability of the ESH test to discriminate between plates of varying susceptibility and to determine EFC rates ii quantitatively. Optical microscopy and analytical TEM were used to investigate the effect of microstructure and local chemistry at grain boundary on EFC susceptibility.
  • Corrosion Resistance of Stainless Steels Presentation Chapter 05: for for Lecturers of Of

    Corrosion Resistance of Stainless Steels Presentation Chapter 05: for for Lecturers of Of

    steels stainless of Supporting presentation for lecturers of resistance Architecture/Civil Engineering Corrosion Chapter 05: Corrosion Resistance of Stainless Steels 1 steels Contents stainless of 1. Most materials decay over time 2. Why does stainless steel resist corrosion resistance 3. Types of corrosion of stainless steels Corrosion Corrosion 4. How to select the right stainless steel for adequate corrosion resistance . Structural applications . Other applications 5. References 2 1. Most Most 1. materials decay over time over 3 Corrosion resistance of stainless steels steels Most materials decay over time stainless of Material Wood Steel Concrete resistance Corrosion Corrosion Type of decay Fungi Rust Cracking/ Insects Spalling Sun+rain Mitigating actions Chemicals Galvanising Corrosion resistant Paint/varnish Painting rebar 4 steels Most materials decay over time stainless of Material Stone Glass Polymers resistance Corrosion Corrosion Type of decay Wear Breaks Become brittle Damage by under UV light Pollution Mitigating actions Usually none taken Tempered glass Improved polymer grades 5 steels Most materials decay over time stainless of Material Aluminum* Copper Stainless resistance Corrosion Corrosion Type of decay Pitting over time, Forms a green No decay possible galvanic patina over time corrosion Mitigating actions Galvanic corrosion None None required can be prevented * Aluminum forms a thin protective oxide just like stainless, but with a much lower corrosion resistance 6 Corrosion in concrete steels (corrosion problems are not limited to outside surfaces !) stainless of . Corrosion of unprotected carbon steel occurs even inside reinforced concrete structures as chlorides resistance present in the environment (marine/deicing) diffuse through the concrete. Corrosion Corrosion . Corrosion products (rust) have a higher volume than the metal, Stainless steel create internal tensions causing the provides both strength concrete cover to spall.
  • A Study on Effect of Intergranular Corrosion by Heat Input on Inconel 625 Overlay Weld Metal

    A Study on Effect of Intergranular Corrosion by Heat Input on Inconel 625 Overlay Weld Metal

    Int. J. Electrochem. Sci., 10 (2015) 6454 - 6464 International Journal of ELECTROCHEMICAL SCIENCE www.electrochemsci.org A Study on Effect of Intergranular Corrosion by Heat Input on Inconel 625 Overlay Weld Metal Joon-Suk Kim1 and Hae-Woo Lee1,* Department of Metallurgical Engineering, College of Engineering, Dong-A University, Busan, 604- 714, Republic of Korea *E-mail: [email protected], Received: 4 May 2015 / Accepted: 31 May 2015 / Published: 24 June 2015 This study discusses the effect of welding heat input on intergranular corrosion of the weld metal of Inconel 625 alloy. A specimen of Inconel 625 overlay with a weld metal that controlled welding heat input was manufactured, and aging heat treatment was conducted to investigate sensitization by chromium carbides. The electrochemical single-loop (SL) and double-loop (DL) electrochemical potentiokinetic reactivation (EPR) experiments, together with the chemical ferric sulfate-sulfuric acid and nitric acid tests, were conducted to determine intergranular corrosion susceptibility between the specimens. In the SL and DL EPR experiments, specimens were stabilized in the weld metal, and therefore intergranular corrosion susceptibility could not be determined. However, in the ferric sulfate- sulfuric acid and nitric acid tests, the corrosion speed increased as heat input increased. This was because the amount of diluted Fe increased as the welding heat input increased, leading to microsegregation between the dendrites, which had a negative effect on the corrosion resistance. Keywords: Inconel 625, Welding, Overlay, Heat input, Intergranular corrosion. 1. INTRODUCTION Inconel 625, which is a Ni-base alloy, is a super heat-resistant alloy that has excellent mechanical properties under high-temperature conditions and high corrosion resistance.