Saudi Aramco Product Specification
Total Page:16
File Type:pdf, Size:1020Kb
Saudi Aramco Product Specification
Number : A-888 Issue Date : 10 Mar 98 Replaces : 28 Oct 96 Page No. : 1 of 2
Test Guarantee Method Ash wt % Max 0.01 ASTM D-482 or P8 5257 Carbon Risidue, 10 % ASTM D-524 or Max 0.35 Bottoms, wt % PS 5252 Cold Flow Properties C (F) Either Cloud Point Winter Nov – Feb Max + 2 (36) Intermediate Oct & Mar Max + 6 (43) ASTM D-2500 Summer Apr – Sep Max + 12 (54) or ISO 3015 Or Cold Filter Plugging Point Max - 4 (25) Winter Nov – Feb Max 0 (32) IP-309 Intermediate Oct & Mar Max + 6 (43) Summer Apr – Sep And Max 10 (18) Difference betwwen Cloud (Note c) Point and CFPP Color Max 3.0 ASTM D-1500 or PS 5067 Corrosion Cu strip, 3 hrs @ Max #. 3 ASTM D-130 or SSA-181 50C (122C) Cetane Index Min 45 ASTM D-976 IP-218 or PS 3 Distillation (% Recovered) ASTM D-86 or ASTM D- 85% Point C (F) Max 350 (662) 2887* ( *in conjunction with End Point To be reported ASTM D-86 correlation ) ASTM D-4294, ASTM D- Sulfur, wt % Max. 1.0 (Note e) 129, ASTM D-1266 (Note D) ASTM D-1552 or PS 5205 Saudi Aramco Product Specification
Number : A-888 Issue Date : 10 Mar 98 Replaces : 28 Oct 96 Page No. : 2 of 2
Test Guarantee Method ASTM D-93 or ASTM D-93 Flash, P. M. Closed, C (F) Min 55 (131) Auto Flash Tester or PS 5260 Gravity, API ASTM D-287, ASTM D-4052 To be reported Specific, 60 , F/60 F or PS 4074
Viscosity: (Min – Max) cSt @ 40C or 1.9 – 4.1 ASTM D-445 32.6 – 40.1 ASTM D-88 or SSA-126 SUS @ 104F
Water and Sediment by Max 0.05 ASTM D-1796 or PS 5253 Centrifuge Vol %
Notes:
a) The PS-Test methods are proposed SASO methods. These will be changed to SSA numbers when they are given final approval by SASO.
b) Targets for Cold Flow Properties are based on Analysis of Diesel Cold Flow Properties: Specification Target Setting, P&CSD/PED-L197/95, April 11, 1995.
c) The 10 C (18 F) maximum margin specification applies only when the CFPP is being used as the primary method in conjunction with the injection of cloud point supressant chemicals. The 10 C (18 F) maximum margin specification is calculated between the CFPP spec and the actual cloud point test.
d) This method is applicable to low sulfur content ( less than 0.4% by Weight )
e) Saudi Aramco guarantees only two significant figures ( 1.0 wt % ) for sulfur. The third figure (1.0X % ) will be rounded off to the nearest number. For example, reported Sulfur results of 1.04 wt % and 1.05 wt % will be considered as ON-SPEC and OFF-SPEC, respectively since 1.04 wt % will be rounded off to 1.0 wt % 1.05 wt % will be rounded off to 1.1 wt %.
f) The rounding off technique is applicable to all Saudi Aramco Product Specifications to the nearest significant figure, similar to the example in note e.